1280 M
Download this page
As
[PDF]
EN 499
E -42 3 B 42 H10
DIN 1913
E 51 54 B H 10
AWS/ASME SFA-5.1 E 7018-H8
Application / Properties:
Electrode for producing
crack- free and tough
welding joints, Weld metal
recovery is approx. 115% .
Smooth and clean welds
blending into base metal
without undercut. Good gap
bridging properties.Owing to
its double covering (up to
3.25mmǾ)
the electrode has a stable
and concentrated arc is
therefore ideally suited for
root pass and positional
welding. Welds are X-ray
quality. Suitable for
depositing layer on steels
having higher carbon Content
(up to .4).
Weld metal analysis in %
(typical values):
|
C |
Mn |
Si |
S |
P |
|
|
0.07 |
1.10 |
0.50 |
0.02> |
0.02> |
|
Mechanical Properties of
all-weld metal :
(single values are typical
values)
|
Yield Strength
(N/mm2) |
Tensile Strength
(N/mm2) |
Elongation
A5(%) |
ISO-V Impact
energy (j)
+200C
-300C |
|
|
>420 |
500-610 |
>22 |
150
70 |
|
|
Amperage: |
|
|
2.5Ǿ |
3.25 Ǿ |
4.0Ǿ |
5.0Ǿ |
6.0Ǿ |
|
|
65-90 |
100-140 |
140-190 |
190-250 |
260-340 |
|
Materials:
|
Unalloyed Structural
steels |
St
33
,St
37,St
44,
St 52-3, St 52-2
|
|
Boiler plates |
H l,H ll,
17 Mn 4 ,19Mn 5
|
|
Pipe steels |
St 35.8,St 37.0,St
37.4,USt 37.0,St
44.0,St 44.4,St 45.8
St 52.0,St 52.4,StE
210.7,StE 290.7,StE
320.0,StE 320.0,StE
360.
Inclouding
corresponding-TM-grades |
|
Fine grain
structural steels |
StE 255, StE 285, StE
315, StE 355
WStE 255, WStE 285,WStE
315,WStE 355 |
|
Shipbuilding steels |
A,B,D,E |
|
cast steels |
GS-38 toGs-52
|
|
|

Redrying : required