1245 N
Download this page
As
[PDF]
DIN 8575 E
CrMo 2 B 26
PrEN 1599
E CrMo 1 B 32 H10
AWS/ASME
SFA-5.5
E 9018 - B 3-H8
Application / Properties:
Electrode for welding of
creep resistant and
high-pressure hydrogen
resistant steels used in the
construction of pressure
vessels, boilers and piping
subjected to operating
temperatures up
to+600C.Owing to its double
covering (up to 3.25mmǾ),
the electrode shows a stable
and concentrate arc, thus
being well suited for root
pass and positional welding
. weld are of X-ray quality.
Preheating, inter-pass
temperature and post-weld
heat treatment in accordance
with base metal to be
welded.
Weld metal analysis in %
(typical values):
|
C |
Mn |
Si |
Cr |
Mo |
|
|
0.06 |
0.80 |
0.50 |
2.40 |
1.00 |
|
Mechanical Properties of
all-weld metal :
(single values are typical
values)
|
|
Yield Strength
(N/mm2) |
Tensile Strength
(N/mm2) |
Elongation
A5(%) |
ISO-V Impact
energy (j)
+200C |
|
|
T
T+N
|
>440
>350
|
570-670
500-600 |
>22
>24 |
100
140 |
|
T
: tempered 0.5 h at
700C,air cooling
T+N
: normalized + tempered
0.5 h at 920C, air cooling
+0.5 h at 750C
|
Amperage: |
|
|
2.5Ǿ |
3.25 Ǿ |
4.0Ǿ |
5.0Ǿ |
|
|
50-85 |
85-130 |
90-180 |
150-240 |
|
Materials:
|
Creep and
high-pressure hydrogen
resistant
steels e.g |
10 CrMo 9 10, 12 CrMo 9 10,
10 CrSiMo V 7, 24 CrMo 10,
GS-12 CrMo 9 10
GS-19 CrMo 9 10 as well as
similar cementation and heat
treatable steels with up to
2% Cr.
|
|
|

Redrying : required
at 300°C to 350°C for 2hrs.
|